摘 要:稀土离子虽然有他本身独特的发光性能,但是他只能吸收很少的激发能量,以至于发光并不理想,有一些配体的吸光系数很高,如果把这两者结合在一起各取所长并相互促进形成发光很好的稀土配合物,这样将会进一步的增加稀土离子的价值和使用率。本文采用最早用于制备稀土复合物的方法:溶胶-凝胶法来制备稀土配合物,采用X射线衍射仪、热比重分析、红外光谱仪等仪器对所制样品进行表征分析。82130
毕业论文关键词:发光性能;荧光;稀土配合物
Synthesis and Luminescence Properties of Rare Earth Composite
Abstract: Although rare earth ions has his own unique luminescent properties, but he can only absorb a small excitation energy, so that the light emission is not ideal, there is a high number of ligand absorption coefficient, if put together from each of the two long and mutually promote the formation of complexes of rare earth luminescent well, this will further increase the value and utilization of rare earth ions。 Prepared rare earth complexes gel method using X-ray diffraction, the proportion of thermal analysis, infrared spectroscopy and other instruments to the prepared samples were characterized by analysis - Sol: In this paper, the method was first used in the preparation of rare earth complexes。
Key Words: Luminescence; Fluorescence; Rare Earth Complexes; Infrared
目 录
摘 要 1
引 言 1
1 实验部分 3
1。1仪器与试剂 4
2 EDTMP-Eu的制备及数据分析 4
2。1 EDTMP-Eu的制备 4
3 EDTMP-Eu的结构分析 4
3。1 红外光谱分析 4
3。2 荧光光谱分析 5
3。3 X射线衍射(XRD)谱图分析 6
3。4 TG曲线分析 7
4 EDTMP-Tb的制备及数据分析 7
4。1 EDTMP-Tb的制备 7
5 EDTMP-Tb的结构分析 8
5。1 红外光谱分析 8
5。2 荧光光谱分析 8
5。3 X射线衍射(XRD)谱图分析 10
5。4 TG曲线分析 10
6 实验总结 10
参考文献 11
致 谢 13
稀土复合材料的合成及发光性能引 言
稀土元素一致的被世界公认为“工业维生素”,稀土体系包括目前使用的元素周期表中第四周期第Ⅲ B族的21号钪 (Sc) 元素、第五周期第Ⅲ B族的39号钇 (Y) 元素和包括镧系在内的所有元素共17个元素[1],稀土元素因为具有独特的未排满的4f电子层,在正三价的电子层组态中他就拥有大量的能级,当某一种物质因为受到外界能量激发 (射线、外电场、高能粒子、电子束等) 时,物质因为得到外界所给的能量将处于某种激发状态,激发态因为拥有较高的能量而处于一种不稳定的状态,物质要趋于稳定就必须处于低能量状态所以一般会以光或热的形式释放出多余的能量,如果释放出的能量位于可见光、紫外光或者是近红外光的电磁辐射范围内时,此过程就可以被称之为发光过程。换句话说,物质除了发生热辐射外还会以其他方式释放出使他处于不稳定态的能量,当以光的方式辐射时就叫做发光过程,一般此过程都会维持一段时间。稀土离子拥有独特的发光性能:很窄的吸收谱带,颜色纯正鲜艳;荧光寿命较长;特征发射波长相对稳定,不容易受到如温度等其他因素的影响;温度和浓度猝灭小[2]。 稀土复合材料的合成及发光性能:http://www.youerw.com/huaxue/lunwen_96268.html