摘 要:凹凸棒石(简称凹土),是一种层链状结构的含水富镁铝硅酸盐粘土矿物。凹土原矿石含有大量的杂质,影响着凹土的使用性能,为了提高其使用效果,不得不对其进行提纯和改性。本课题利用硅烷偶联剂(MPS)对凹土进行改性,使其表面富含碳碳双键,然后在引发剂过硫酸钾(KPS)的作用下,采用自由基聚合法在改性凹土表面接枝PDMAEMA,制备改性凹土(PGS-g-PDMAEMA),通过红外光谱分析(FTIR)、X射线衍射图谱(XRD)、X射线光电子能谱(XPS)和热重分析(TG)对其进行表征。结果表明,PDMEAMA已成功接枝于PGS-MPS上,且最佳的单体用量为4 g,此时接枝率为8。48 %。85719
毕业论文关键词:聚甲基丙烯酸-N,N-二甲氨基乙酯,凹土,硅烷偶联剂,接枝
Abstract: Palygorskite (PGS) is crystal hydrated magnesium aluminum silicate with a unique layer-chain structure。 The raw ore of PGS contain a large amount of impurities, which affect the service performance。 We need to purify and modify it to improve its use。 Modified palygorskite was synthesized via grafting poly [2-(N,N-dimethyl amino)-ethyl methacrylate]。 Potassium sulphate (KPS) was the initiator, and coupling agent (MPS) made surface rich in Carbon-Carbon Double Bond。 The copolymer was successfully cast via free radical polymerization。 It was characterized by infrared spectrum (FTIR), X-ray diffraction patterns (XRD), X-ray photoelectron spectroscopy (XPS), and thermogravimetric analysis (TG)。 The results showed that PDMEAMA was successfully grafted on PGS-MPS。 The optimum monomer dosage was 4 g, while the graft rate was 8。48 %。
Keywords: poly [2-(N,N-dimethyl amino)-ethyl methacrylate], palygorskite, silane coupling agent, graft
目 录
1 引言 …4
1。1 凹土的结构 4
1。2 凹土的应用 4
1。3 凹土的改性源Q于W优H尔J论K文M网WwW.youeRw.com 原文+QQ75201.,8766 方法 5
1。4 研究的目的与意义 6
2 实验部分 6
2。1 实验药品和仪器 6
2。2 改性凹土的制备 7
2。3 凹土的表征 8
3 结果与讨论 9
3。1 红外光谱分析(FTIR) 9
3。2 X射线衍射图谱分析(XRD) 10
3。3 X射线光电子能谱分析(XPS) 11
3。4 热重分析(TG) 12
结 论 14
参 考 文 献 15
致 谢 17
1 引言
1。1 凹土的结构来自优W尔Y论W文C网WWw.YoueRw.com 加QQ7520,18766
凹凸棒石(简称凹土),是一种层链状结构的含水富镁铝硅酸盐粘土矿物[1],其晶体结构示意图见图1-1。它的晶体基本构造可分成三个层次[2]:一是凹土的基本构造单元,也就是棒状单晶体;二是通过棒晶与棒晶之间彼此靠近堆积而形成棒晶束;三是通过棒晶束之间层层累积而形成的不同聚合体。凹土的理想晶体化学式Mg5(Si8O20)(OH)2(OH2)4·4H2O,其理论化学成分SiO2 56。96 %,MgO 23。83 %,H2O 19。21 %。
图1-1 凹土晶体结构示意图
1。2 凹土的应用